    The C40 super fine sand concrete is produced by using Handan local material and the influ-ence of water-binder ratio, fly ash replacement rate, and sand ratio on the 28 d compressive strengthand workability are studied in orthogonal experiment design.The results show that fly ash replacementis the most primary factor effecting on 28 d compressive strength and sand ratio is the most primaryfactor effecting on workability.Appropriate fly ash replacement can improve the 28 d compressivestrength.With the increase of sand ratio, slumps decrease sharply and strength decreases slightly.Itcalls for using the 0.45 as water-binder ratio, 10% as fly ash replacement and 30% as sand ratio tomake reasonable design of mix proportions, we can obtain the super fine concrete strength that its 28d compressive strength reaches to 59.1 MPa, for 60mm of slump.

    Reference
    Related
    Cited by
Get Citation

HE Jin-yun, WANG Lu-lu. Study on the workability and compressive strength of C40 superfine sand concrete[J].,2012,29(3):1-4,10

Copy
Related Videos

Share
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:August 21,2012
  • Revised:
  • Adopted:
  • Online: January 12,2015
  • Published:
Article QR Code